- La description
- Enquête
Plastic Granules Based Thermoplastic Rubber TPR Sole Material Supplier Wholesale in China.
WINIW supply high quality TPR material for shoe soles, TPR shoe sole material, plastic granules thermoplastic rubber raw materials for shoe soles manufacturing. Prix de haute qualité et compétitif!
Commodity | TPR | Quality inspection date | ||||
No. | Article | Unit | Standard | Determine scope | Testing result | Test method |
1 | Apparence | Visual test | Natural color | Natural color | ||
2 | Dureté | Shore A | ASTM-D2240 | 0~100 | 30C | indoor temperature℃ |
3 | Density | SP.Gr | ASTM-792 | 1.15±0.05 | 1.2 | |
4 | Solution flow index | g/10min | ASTM-D1238 | 5~20 | 13 | 190℃,2.16kg |
5 | Résistance à la traction | Mpa | ASTM-D412 | ≥5 | 7.8 | indoor temperature 500mm/min |
6 | Elongation | % | ASTM-D412 | ≥500 | 550 | |
7 | Tear strength | KN/m | ASTM-D624 | ≥20 | 23 | |
Manufacturing technique | ||||||
Barrel temperature | Range ℃ | Typical value ℃ | ||||
Forepart | 150-190 | 170 | ||||
Midpiece | 150-210 | 180 | ||||
Back end | 150-210 | 180 | ||||
Orifice/Die-head | 160-200 | 180 | ||||
Upper limit of processing temperature ℃ | 220 | |||||
Time of drying | Generally there is no need to dry,If the storage environment is humid or the production of products surface requirements higher parts,dry in a hot air oven for 2 à 4 heures | |||||
1.The above data is only for reference. The above data can be adjusted according to different models,molds and product requirements.2.Do not allow the material in the barrel to stay too long too long,Please use PE to clean the machine before stopping it. | ||||||
Materials can be developed and produced according to clients’ requirements |